TRANSMISSION // 2611.33112v1
A titanium seed helps tantalum grow at room temperature
Source published
An ultrathin titanium layer helps stabilize a useful form of tantalum on sapphire at room temperature. Resonator tests show promising microwave performance, while also revealing that growth and cleaning can affect losses.

Superconducting circuits need materials that lose very little energy at microwave frequencies. Tantalum is a promising choice, but producing its desired α phase reliably can be difficult. This study tests whether a near-atomic-thin titanium seed layer can make that growth more forgiving—and whether the resulting films perform well in resonators and a test qubit device.
The challenge: getting the right tantalum phase
Tantalum films can form in different crystal structures. For superconducting circuits, researchers are interested in α-tantalum, but small changes in how a film is deposited can affect which phase forms. The authors investigate whether an ultrathin titanium layer on sapphire can help α-tantalum grow reliably at room temperature, without heating the substrate during deposition.
The team compared titanium-seeded films with tantalum grown at high temperature without a seed layer, and with a room-temperature film using a niobium seed. They examined crystal structure with X-ray diffraction and surface texture with atomic force microscopy. To assess microwave performance, they fabricated coplanar-waveguide (CPW) resonators—structures that guide microwave signals—and measured their internal quality factors at cryogenic temperatures. They also tracked resonator behavior as temperature rose and built a ten-transmon test device using the titanium-seeded film.
A thin seed changes the outcome
Without titanium, room-temperature-grown tantalum was predominantly in the β phase, with traces of α phase. About half a monolayer of titanium produced mixed phases. At approximately one or two monolayers, the films instead showed phase-pure α-tantalum with a strong (110) orientation.
A monolayer is an approximate measure of a single atomic layer’s coverage. The useful titanium thickness was ultrathin, and its upper limit differed between the two sputtering systems tested. With about one monolayer of titanium, α-tantalum persisted across a range of argon sputter-gas flows; the authors observed departures from phase purity at a higher flow. The results suggest the seed layer makes growth less sensitive to settings within the tested window, rather than removing the need to control them.
The titanium-seeded films had a different crystal orientation and surface appearance from the high-temperature-grown reference films. For the compared samples, the reported root-mean-square surface roughness was about 0.73 nm for the seeded α-tantalum (110) film and about 0.39 nm for the heated α-tantalum (111) film. The heated film also showed visible surface features. These particular measurements illustrate why surface roughness alone cannot capture every aspect of film quality.
Resonators test microwave loss
At the lowest temperatures, the researchers measured how resonator loss changed with microwave drive and fitted a model for loss attributed to two-level systems (TLSs). For the optimized titanium-seeded films, the TLS-limited quality factor exceeded 3 million in the widest resonators. Their low-temperature performance was comparable to the high-temperature-grown reference films and to previously reported tantalum resonators with similar geometries.
Temperature-dependent measurements add an important qualification. For the optimized titanium-seeded film, measurements from about 20 millikelvin to 1 kelvin were described by the authors’ TLS and quasiparticle-loss models. Additional temperature-activated loss was seen in the high-temperature-grown films and in one titanium-seeded film subjected to a prolonged buffered-oxide etch (BOE). The tested titanium-seeded films receiving moderate BOE treatment or the optimized cleaning procedure did not show that same behavior.
The extra loss was not explained by the standard TLS and quasiparticle models used in the paper. The authors discuss vortex motion as one possible explanation, but do not establish its cause; magnetic-field-dependent tests and further investigation would be needed. The chemical or structural changes associated with prolonged etching also remain unresolved.
What this means—and what remains open
A ten-transmon device made with the optimized titanium-seeded film had an average qubit relaxation time, T1, of 96 ± 19 microseconds. This demonstrates compatibility with a test device, not that the seed layer alone determines qubit coherence. Processing steps and other loss sources may also contribute.
Overall, the work presents an alternative route to room-temperature α-tantalum growth and shows promising resonator performance. It also indicates that microwave behavior depends on more than crystal phase: growth conditions and post-processing matter, and some loss mechanisms remain unidentified.
The source is an arXiv preprint. The supplied evidence does not establish its peer-review status. The study tests a finite set of films, resonators, deposition conditions, and cleaning procedures, so its comparisons do not establish a universal ranking of seed materials or growth methods. Several authors are listed as inventors on a patent application related to the work. Further independent tests could help determine how broadly the process transfers and clarify the origin of the activated loss.
- tantalum
- superconducting circuits
- titanium seed layer
- thin-film growth
- microwave resonators
- quantum materials
Related reading
Automatically matched by shared topic keywords. These links do not imply that the sources agree or establish a consensus.
What tiny superconductors need to become reliable quantum devices
Source published
Shared keywords: quantum materials
When the Dipole Approximation Misses the Shape of Light
Source published
Shared keywords: quantum materials
Simplifying noise models for superconducting circuits
Source published
Shared keywords: superconducting circuits
Teleporting a logical qubit by joining code patches
Source published
Shared keywords: superconducting circuits
A quieter route to tunable light–matter interactions
Source published
Shared keywords: superconducting circuits